Jowat 150.91PU Dispersion Glue | 91-WHITE & 95-BLUE
Application
PU dispersion with built-in crosslinking mechanism, excellent film formation, high initial
strength and good water and heat resistance after crosslinking. Heat resistance values
are higher if the lamination is carried out within 8 hours after adhesive application.
Min. temp. (materials, glue and room
air):
Glue Application: 15°C (58°F)
Application amount : one sided
Min. activation temp. in the bondline: 2-5 mil wet=5-12 g/sqft (depending on board quality
quality)
Min. activation temp. in the bondline: 55°C (131°F)
Applied by spraying (cup or pressure pot). Pot and gun components must be stainless
steel or plastic. Diameter of spray nozzle should be 1.0-1.5 mm (.040-.060 inches).
The edges should be sprayed a second time after the first coat has dried. Glue film
must be completely dry before pressing. Complete curing at room temperature takes
about 7 days.
Depending on the adhesive, type of foil, foil thickness, design and shape of the MDF part
and test method used, it is possible to achieve heat resistance values between 80 and
100ºC (176 to 212ºF).
Technical Data
Viscosity [mPas]: approx. 3,000 (Brookfield)
Density [g/cm³]: approx. 1.05 (8.7 lbs./gal.)
Solids [%]: approx. 41
pH value: approx. 8
Appearance: 90 - opaque with UV indicator; 91 - white; 95 - blue
| Weight | 49 lbs |
|---|---|
| Dimensions | 15 × 15 × 16 in |
| Color |
blue |
| Packaging |
Buckets |
| Per Box |
1 |
Cleaning
Fresh glue may be removed with cold water. Dried glue must be removed
mechanically.
Storage
May be stored in properly closed original containers, cool and dry (15-25°C (59-77°F)).